Сарымсаков Абдушкур АбдухалиловичInstitute of Polymer Chemistry and Physics of the Academy of Sciences of the Republic of UzbekistanA. I. ShukurovInstitute of Polymer Chemistry and Physics of the Academy of Sciences of the Republic of UzbekistanН. Ш. АшуровInstitute of Polymer Chemistry and Physics of the Academy of Sciences of the Republic of UzbekistanKhaydar E. YunusovInstitute of Polymer Chemistry and Physics of the Academy of Sciences of the Republic of Uzbekistan
ABI
Abstract
The properties of cellulose diacetate solutions in acetone and acetone–water mixtures at ratios of 95:5, 93.5:7.5 and 90:10 were studied. The optimal concentrations of cellulose diacetate solution for the formation of nanofibers from a mixture of water and acetone with a water content of 7.5 wt% were found. Cellulose diacetate nanofibers were obtained in the form of nonwoven materials with an average nanofiber diameter of 350±10 nm. In order to obtain cellulose nanofibers with a thread diameter of 350–400 nm, cellulose diacetate nanofibers were hydrolyzed in a 0.1 M potassium hydroxide solution.
Topics
Identifiers
Citations and references
Cited by 018 references
Metrics — AkademScholar · Coming soon