Thermal degradation of commercially available organoclays studied by TGA–FTIR

José Manuel Cervantes‐UcCentro de Investigación Científica de Yucatán, A.C., Calle 43 No. 130, Col. Chuburná de Hidalgo, C.P. 97200, Mérida, Yucatán, MexicoJuan Valerio Cauich‐RodríguezCentro de Investigación Científica de Yucatán, A.C., Calle 43 No. 130, Col. Chuburná de Hidalgo, C.P. 97200, Mérida, Yucatán, MexicoHumberto Vázquez‐TorresUniversidad Autónoma Metropolitana – Iztapalapa, Departamento de Física, San Rafael Atlixco No. 186, Col. Vicentina, C.P. 09340, México D.F., MexicoL. F. Garfias‐MesiasRD&E, Corrosion Laboratory, S. C. Johnson & Son, Inc., 1525 Howe Street, M/S #051, Racine, WI 53403, USADonald R. PaulDepartment of Chemical Engineering and Texas Materials Institute, University of Texas at Austin, TX 78712, USA
2007en