Г. І. КириченкоB. I. Verkin Physicotechnical Institute of Low Temperatures, Ukrainian Academy of Sciences, KharkovВ. Д. НацикB. I. Verkin Physicotechnical Institute of Low Temperatures, Ukrainian Academy of Sciences, KharkovV. P. SoldatovB. I. Verkin Physicotechnical Institute of Low Temperatures, Ukrainian Academy of Sciences, Kharkov
ABI

Аннотация

Work-hardening curves are obtained for Sn–Cd alloys with Cd concentrations 0.01, 0.21, and 0.53 at.% in the temperature interval 4.2–100 K. The impurity is found to have a noticeable temperature-dependent effect on the work-hardening curves. The temperature dependences of the yield stress and the duration of the easy slip stage are also determined.