Study of the properties of asphalt concrete based on solid waste from cement production
G B IbrokhimovTermez Institute of Engineering and Technology, 288b, Islam Karimov Avenue, Termez, 190111, UzbekistanJ L ShukurovTermez Institute of Engineering and Technology, 288b, Islam Karimov Avenue, Termez, 190111, UzbekistanCh A KhasanovTermez Institute of Engineering and Technology, 288b, Islam Karimov Avenue, Termez, 190111, UzbekistanS S OmondavlatovTermez Institute of Engineering and Technology, 288b, Islam Karimov Avenue, Termez, 190111, UzbekistanI E TovosharevaTermez Institute of Engineering and Technology, 288b, Islam Karimov Avenue, Termez, 190111, Uzbekistan
ABI
Аннотация
Abstract It is known that in the production of cement, clinker is treated at a temperature of 1350-1400 C°. During this process, slag is formed in the furnace. In addition, dispersed cement dust accumulates in dust retention filters. One of the ways to effectively use them is to use them as fillers or modifiers in the production of various composite materials. After special processing, the possibility of using these wastes as a modifying filler in increasing the strength of asphalt concrete compositions was studied.
Ҳали таржима қилинмаган
Мавзулар
Идентификаторлар
Иқтибослар ва манбалар
0 та иқтибос3 та фойдаланилган манба
Кўрсаткичлар — AkademScholar · Тез орада