Properties of cotton/polyester composite ring spun yarns

Shavkat FayzullaevTashkent Insititute of Textile and Light Industry, Tashkent, UzbekistanHusanhon BobojanovNamangan Institute of Engineering and Technology, Namangan, UzbekistanSaypila MatismailovTashkent Insititute of Textile and Light Industry, Tashkent, UzbekistanDoniyor ParpievNamangan Institute of Engineering and Technology, Namangan, Uzbekistan
ABI

Аннотация

The article presents the results of the analysis of the properties of composite yarns spun in the cotton/polyester ring method. For this, samples were prepared in the proportions of 15.4 tex (Ne 40/1) 80/20%, 60/40%, 50/50%, and 0/100%. Samples of mixed yarns were made using medium-fiber cotton fiber (linear density 0.186 tex×length 32 mm) and polyester fiber (linear density 0.164tex×length 38 mm). Unevenness in the mass of finished yarns, thin and thick places, the number of neps, specific tensile strength, tensile strength, breaking work (B-work) were determined using USTER test instruments (Uster® Tester 6, Uster® Tensojet 4, etc.) and obtained. The parameters were checked for compliance with the Uster® Statistics 2018. The increase in the proportion of polyester fibers in mixed yarns has led to a decrease in the mass unevenness of the yarn, thin and thick places, and the number of neps; on the other hand, the specific tensile strength of the yarn, the tensile strength, the breaking work values of the yarn increased.

Ҳали таржима қилинмаган

Мавзулар

Идентификаторлар

Иқтибослар ва манбалар