Structural, morphological, optical, and electrical properties of SbxSey films with different compositions grown by Chemical-molecular beam deposition method from Separate Sb and Se precursors
T.M. RazykovPhysical-Technical Institute, Chingiz Aytmatov Street 2B, 100084, Tashkent, UzbekistanK.M. KouchkarovPhysical-Technical Institute, Chingiz Aytmatov Street 2B, 100084, Tashkent, UzbekistanB. A. ErgashevPhysical-Technical Institute, Chingiz Aytmatov Street 2B, 100084, Tashkent, UzbekistanР. ХуррамовPhysical-Technical Institute, Chingiz Aytmatov Street 2B, 100084, Tashkent, UzbekistanD. Z. IsakovPhysical-Technical Institute, Chingiz Aytmatov Street 2B, 100084, Tashkent, UzbekistanМ. С. ТивановFaculty of Physics, Belarusian State University, Nezavisimosti Ave. 4, 220030, Minsk, Belarus
ABI
Аннотация
Аннотация мавжуд эмас.
Мавзулар
Идентификаторлар
Иқтибослар ва манбалар
0 та иқтибос30 та фойдаланилган манба