Features of Hydride Synthesis

M. S. PaizullakhanovInstitute of Materials Science, Academy of Sciences of the Republic of Uzbekistan, Tashkent, UzbekistanO. R. ParpievInstitute of Materials Science, Academy of Sciences of the Republic of Uzbekistan, Tashkent, UzbekistanE. Z. NodirmatovInstitute of Materials Science, Academy of Sciences of the Republic of Uzbekistan, Tashkent, Uzbekistan
Chemical Reportsjournal2026
ABI

Аннотация

Lithium, sodium, and titanium hydrides have been synthesized. It has been found that lithium hydride is formed at a temperature of 650-700°C and a pressure of 12 atm. Lithium hydride contains 11 mass.% of hydrogen. Hydrogen desorption from lithium hydride occurs at a temperature of 700°C. Lithium hydride decomposes in water to form lithium hydroxide and hydrogen. Sodium hydride is formed at a temperature of 300-450°C with a hydrogen absorption level of up to 4 mass%. Hydrogen desorption from sodium hydride occurs at a temperature of 350-400°C. Titanium hydride is formed at a temperature of 600-650°C with a hydrogen absorption level of up to 4 mass%. Hydrogen desorption from sodium hydride occurs at a temperature of 450-650°C. Lithium, sodium, and titanium hydrides can be used in hydrogen storage and transportation processes.

Ҳали таржима қилинмаган

Мавзулар

Идентификаторлар

Иқтибослар ва манбалар