POLYMER RESIN PRODUCTION FROM PYROLYSIS PRODUCTS: PROCESS PARAMETERS AND SOLUBILITY ANALYSIS
Ziyadullayev Anvar EgamberdiyevichTashkent Chemical-Technological Institute, Uzbekistan, TashkentSuvonqul NurmanovDepartment of chemistry of the National University of Uzbekistan, Republic of Uzbekistan, TashkentJonibek NuriddinovTashkent Chemical-Technological Institute, Uzbekistan, TashkentOrifjon QodirovNational University of Uzbekistan, Uzbekistan, Tashkent
2025en
Ochiq kirishOlmos
ABI
Annotatsiya
This study investigates the physico-chemical properties and the potential for producing petroleum polymer resins from secondary oil pyrolysis products - distillates, condensates, and heavy fractions obtained at the Ustyurt gas-chemical complex. Pyrolysis was carried out at temperatures ranging from 120 to 230 °C for 1 to 4 hours. The products were separated into gas, liquid, and resin fractions, and their density, viscosity, thermal stability, and elemental composition were analyzed. The optimal conditions for resin extraction from the heavy fraction were found to be a temperature of 180–200 °C and duration of 3 hours.
Hali tarjima qilinmagan
Identifikatorlar
Iqtiboslar va manbalar
0 ta iqtibos0 ta foydalanilgan manba