Asosiy kontentga oʻtish
Maqola

High-Temperature Quenching and Combined Heat and Chemical-Thermal Treatment of Heat-Resistant Die Steels and High-Speed Steel R6M5

J. M. BegatovM.S. ErgashevM.M. PlatoshinaKimyo International University in Tashkent
2026en
ABI

Annotatsiya

The effect of the quenching temperature, tempering and low-temperature cyanidation (nitrocarburizing) on the structure, heat resistance and wear of the heat-resistant die steels 4KhMFS, 4Kh5MF1S and 3Kh2V8F and the high-speed steel R6M5 was investigated with the aim of developing combined hardening technologies. Raising the quenching temperature from 1050 to 1150–1200 °C increases the dislocation density of the martensite, which reaches about 3.4·1011 cm−2 in as-quenched steel 4KhMFS, the austenite grain size grows from 0.025–0.032 to 0.044–0.047 mm, and the heat resistance of steel 4KhMFS (HRC 45 criterion) increases from 550 to 620 °C. Steel 3Kh2V8F quenched from 1150 °C retains HRC 50 up to 670 °C; its wear has a minimum of 0.29 mm after tempering at 600 °C, where the dislocation density increases due to precipitation of dispersed alloy carbides, and a linear regression L = 0.778 – 0.285x (R2 = 0.97) relates the wear to the dislocation density. Cyanidation in a solid mixture of carbon black and urea at 550–600 °C for 1–4 h, which coincides with the tempering range, forms carbonitride layers 0.05–0.20 mm deep with a surface microhardness of 8000–12000 MPa; the layers remain harder than the core after thermal cycling between 150 and 750 °C. The combined treatment of a drawing drum band surfaced with 3Kh2V8F wire increased its service life from about 0.8 to 3 t of drawn wire, and combining cyanidation with a one-hour tempering at 600–610 °C increased the life of R6M5 cutters by 1.4–1.5 times while shortening the hardening cycle.

Hali tarjima qilinmagan

Iqtiboslar va manbalar