COMPREHENSIVE STUDIES OF CERAMIC BRICK WASTE AS A RAW MATERIAL COMPONENT FOR PRODUCING PORTLAND CEMENT CLINKER
Annotatsiya
The paper presents information on the results of research to determine the possibility of using waste from the production of ceramic bricks instead of natural clay raw materials as an aluminosilicate component of the raw mixture for firing clinker. The process of chemical interaction of the components proceeds intensively, the assimilation of CaO free during firing of charge No. 1 is practically completed at a temperature of (1350-1380) 0 C, and of charge No. 2 at (1380-1400) 0 C with the complete formation of clinker minerals. The content of CaO free in them does not exceed (no more than 1.0%) the standard value. It is noted that the new raw material mixtures are characterized by high reactivity and provide the synthesis of clinker with a good structure at a temperature 50-80°C lower than that of mixtures with natural clay raw materials - loess-like rock.
Hali tarjima qilinmagan