Does Hydroxyapatite Reinforce Conventional Glass Ionomer Cements? A Systematic Review of In Vitro Evidence on Mechanical Properties

Malokhat PatkhiddinovaDepartment of Restorative Dentistry, Faculty of Dentistry, Universiti Malaya, Kuala Lumpur, MalaysiaJaloliddin PatkhiddinovDepartment of Orthodontics Paediatric and Special Care Dentistry, Faculty of Dentistry, Universiti Malaya, Kuala Lumpur, MalaysiaRana DiabDepartment of Restorative Dentistry, Faculty of Dentistry, Universiti Malaya, Kuala Lumpur, MalaysiaAnas Hakimee Ahmad UbaidillahDepartment of Restorative Dentistry, Faculty of Dentistry, Universiti Malaya, Kuala Lumpur, MalaysiaZohaib KhurshidDepartment of Oral and Maxillofacial Surgery, Biruni University, Istanbul, TurkeyS. H. YusupalikhodjaevaDepartment of Propaedeutic Therapeutic Dentistry, Tashkent State Medical University, Tashkent, UzbekistanNoor Azlin YahyaDepartment of Conservative Dentistry, Faculty of Dental Medicine, Universitas Airlangga, Surabaya, Indonesia
2026en
Ochiq kirishOltin

Litsenziya: cc-by

ABI

Annotatsiya

Background: This systematic review evaluated the effects of hydroxyapatite (HA), as the sole added filler, on the mechanical properties of conventional glass ionomer cements (GICs). Methods: PubMed/MEDLINE, Scopus, Web of Science, EBSCOhost and Google Scholar were searched up to 13 July 2026 following PRISMA 2020 (PROSPERO CRD420251079759). Two reviewers independently performed study selection, data extraction and risk-of-bias assessment using RoBDEMAT. Heterogeneity in HA characteristics, concentration, powder-to-liquid ratio and testing protocols precluded meta-analysis. Results: of 1816 records identified, 22 studies met the eligibility criteria. Compressive strength was higher than that of the unmodified cement in 6 of 13 studies, lower in 4 and unchanged in 3. Flexural strength was higher in 6 of 7 studies and diametral tensile strength in 3 of 5, in at least one tested formulation. Surface microhardness findings were inconsistent, with higher values in 2 of 6 studies, lower values in 2 and no clear change in 2. Fracture toughness was assessed in a single study. Improvements were most consistent at about 5 wt% HA, but the response varied with particle characteristics and the host cement, and no optimal concentration could be identified. Conclusions: HA effects on GIC mechanical properties depend on formulation and testing conditions.

Hali tarjima qilinmagan

Identifikatorlar

Iqtiboslar va manbalar

0 ta iqtibos0 ta foydalanilgan manba