Contribution of Pearlite, Dislocation Density and Cementite Dispersion to the Abrasive Wear Resistance of Carbon Steels with a Ferritic Matrix

J.M. BegatovM.S. ErgashevM.M. PlatoshinaKimyo International University in Tashkent
2026en
ABI

Annotatsiya

The article quantifies the separate contributions of the main structural parameters of carbon steels with a ferritic matrix to their abrasive wear: the fraction of pearlite, the dislocation density of the α-phase, the carbon dissolved in ferrite and the dispersion of cementite particles expressed through the inter-carbide spacing λ. Armco iron and steels 08kp, 20, 30, 45, 70 and U12 were annealed, normalized or quenched from 870–1200 °C and tempered at 200–600 °C so that one parameter prevailed while the others were kept nearly constant. Wear was measured on an X4-B machine against a fixed abrasive, the dislocation density was calculated from the physical broadening of the (220) X-ray line, and λ was determined on carbon replicas. In the annealed state the wear decreases from 0.88 mm (Armco iron) to 0.60 mm (steel 70) as the pearlite fraction increases from 0 to 94 %, following ΔL = 0.275√P. The dislocation density of ferrite reaches a maximum after heating to 1100 °C, and the wear decreases linearly with √ρ with a coefficient of about 0.12 mm per 105 cm−1. Carbon in ferrite lowers the wear by 1.143 mm per 1 wt.% C, and cementite particles by ΔL = S/λ, where S equals 0.178, 0.04 and 0.015 mm·µm after tempering at about 600, 400 and 300 °C. As strength grows, the sensitivity of wear to every structural parameter decreases. The obtained additive relation forms a quantitative basis for choosing steels and hardening modes.

Hali tarjima qilinmagan

Iqtiboslar va manbalar