OBTAINING AND PROPERTIES GRAFT COPOLYMERS OF DIALDEHYDE CARBOXYMETHYLCELLULOSE/SERICINE
Annotatsiya
In this article, research work on obtaining graft copolymers based on dialdehyde carboxymethylcellulose (DCMC) with a molecular weight of 141 kDa, oxidation degree of 82% and sericin with a molecular weight of 180 kDa and study their physics-chemical properties. The functional groups in the obtained DCMC/sericin graft copolymers were analyzed by infrared (IR) and nuclear magnetic resonance (NMR) spectroscopy methods. It was observed that the sorption and physical-mechanical properties of DCMC-sericin graft copolymers increased compared to the initial samples. It was found that DCMC, sericin, DCMC-sericin graft copolymers absorbed water vapor in the amount of 8, 9, 13 mmol/g, respectively. Based on the sorption properties, the value of Gibbs energy was calculated to study the polymer-solvent effect.
Hali tarjima qilinmagan