A criterion of contamination of the glass surface of photovoltaic batteries

М. Н. ТурсуновPhysics–Sun Physicotechnical Institute, Uzbekistan Academy of Sciences, Tashkent, UzbekistanВ. Г. ДыскинAcademy of Sciences Republic of UzbekistanI. A. YuldashevPhysics–Sun Physicotechnical Institute, Uzbekistan Academy of Sciences, Tashkent, UzbekistanKh. A. SobirovPhysicotechnical InstitutePark Jeong Hwoan
Applied Solar Energyjournal2015en

Ochiq kirish: yoʻq

ABI

Annotatsiya

The relative change in the coefficient of efficiency is chosen as a criterion for contamination of the glass surface of a photovoltaic battery. Using the formula obtained, the results of measurements of the transmission coefficient of a contaminated glass plate after its exposure to open air in the center of Tashkent for 80 and 110 days are processed. It is shown that the contamination of the glass plate reduces the coefficient of efficiency of the PVB by 50.0%.