TGA-BASED THERMAL STABILITY AND OXYGEN-INDEX PREDICTION OF AN EPOXY-COAL TAR COATING
Annotatsiya
Summary. A mineral-filled epoxy-coal tar protective coating was evaluated by re-analysis of an existing thermogravimetric record and by a transparent, TGA-based oxygen-index screening calculation. The coating consists of an ED-20 epoxy resin/coal tar binder, DTB-2 hardener, furfuryl alcohol distillation residue, wollastonite, andesit0e flour and saponified tall pitch. The thermogravimetric record shows only limited mass change below approximately 150 °C, followed by the principal degradation interval at about 150–330 °C. The specimen mass decreases from approximately 8.2 mg to 2.6–2.7 mg after the main decomposition stage. A near-plateau is observedbetween about 330 and 430 °C, followed by slower secondary mass loss. At approximately 700 °C, 1.6–1.7 mg remains, corresponding to 19.5–20.7% of the initial mass. This residual fraction is close to the nominal 21 wt.% content of wollastonite and andesite flour and is therefore compatible with a mineral-dominated high-temperature residue. For preliminary flame-response screening, the historical van Krevelen correlation between high-temperature residue and limiting oxygen index was applied to the available residual-mass range, giving an apparent predicted oxygen index of approximately 25.3–25.8 vol.% (midpoint 25.5 vol.%). Because the residue contains a substantial inorganic fraction and the original TGA atmosphere was not reported, this value is presented only as a model-based screening estimate and not as an experimental oxygen-index result. Direct testing according to ISO 4589-2 or ASTM D2863 remains necessary for a quantitative flammability claim.
Hali tarjima qilinmagan