Comparison of laser induced thermal fracture between polycrystalline ceramic and crystal Nd:YAG

Yu ShenResearch Center for Laser Physics and Technology, Key Lab of Functional Crystal and Laser Technology, Technical Institute of Physics and Chemistry, Chinese Academy of Sciences, Beijing 100190, ChinaWenbin LiuKey Laboratory of Transparent Opto-functional Inorganic Materials, Shanghai Institute of Ceramics, Chinese Academy of Sciences, Shanghai 200050, ChinaNan ZongTechnical Institute of Physics and ChemistryJiang LiKey Laboratory of Transparent Opto-functional Inorganic Materials; Shanghai Institute of Ceramics; Chinese Academy of Sciences; Shanghai 200050 ChinaYong BoResearch Center for Laser Physics and Technology, Key Lab of Functional Crystal and Laser Technology, Technical Institute of Physics and Chemistry, Chinese Academy of Sciences, Beijing 100190, ChinaXiqi FengKey Laboratory of Transparent Opto-functional Inorganic Materials, Shanghai Institute of Ceramics, Chinese Academy of Sciences, Shanghai 200050, ChinaFangqin LiTechnical Institute of Physics and ChemistryYubai PanKey Laboratory of Transparent Opto-functional Inorganic Materials, Shanghai Institute of Ceramics, Chinese Academy of Sciences, Shanghai 200050, ChinaYa-Ding GuoResearch Center for Laser Physics and Technology, Key Lab of Functional Crystal and Laser Technology, Technical Institute of Physics and Chemistry, Chinese Academy of Sciences, Beijing 100190, ChinaPeng‐Yuan WangResearch Center for Laser Physics and Technology, Key Lab of Functional Crystal and Laser Technology, Technical Institute of Physics and Chemistry, Chinese Academy of Sciences, Beijing 100190, ChinaWei TuTechnical Institute of Physics and ChemistryQinjun PengTechnical Institute of Physics and ChemistryJingyuan ZhangResearch Center for Laser Physics and Technology, Key Lab of Functional Crystal and Laser Technology, Technical Institute of Physics and Chemistry, Chinese Academy of Sciences, Beijing 100190, ChinaWenqiang LeiTechnical Institute of Physics and ChemistryDafu CuiResearch Center for Laser Physics and Technology, Key Lab of Functional Crystal and Laser Technology, Technical Institute of Physics and Chemistry, Chinese Academy of Sciences, Beijing 100190, ChinaZuyan XuTechnical Institute of Physics and Chemistry
2014en
ABI

Annotatsiya

Continuous wave 808 nm pump laser-induced thermal damage of polycrystalline transparent ceramic and crystalline Nd:YAG materials was investigated both experimentally and theoretically. The measured temperature agrees well with the theoretical simulation, and the maximum hoop stresses occur on the incident facet of the end-pumped rod at about √2 times of the pump beam radius w0, where the temperature gradient is the highest and the damage occurs first at this location. The fracture-limited laser intensity of ceramics was experimentally measured to be 6.4±0.6 kW/cm2, nearly 64% higher than that of the crystals (3.9±0.3 kW/cm2). The deduced thermal fracture stress for ceramic was 386±50 MPa, which is 64% higher than that of the crystals (235±16 MPa).

Hali tarjima qilinmagan

Identifikatorlar

Iqtiboslar va manbalar

3 ta iqtibos0 ta foydalanilgan manba