Annealing behaviors of photoluminescence from SiOx:H

Zhixun MaState Laboratory for Surface Physics, Institute of Semiconductors, Center for Condensed Matter Physics, Chinese Academy of Sciences, P.O. Box 912, Beijing 10083, ChinaXianbo LiaoInstitute of SemiconductorsJie HeInstitute of SemiconductorsWenchao ChengState Laboratory for Superlattices and Microstructures, Institute of Semiconductors, Chinese Academy of Sciences, P.O. Box 912, Beijing 100083, ChinaGuozhen YueInstitute of SemiconductorsYongqian WangState Laboratory for Surface Physics, Institute of Semiconductors, Center for Condensed Matter Physics, Chinese Academy of Sciences, P.O. Box 912, Beijing 100083, ChinaGuanglin KongState Laboratory for Surface Physics, Institute of Semiconductors, Center for Condensed Matter Physics, Chinese Academy of Sciences, P.O. Box 912, Beijing 100083, China
1998en
ABI

Annotatsiya

The strong photoluminescence (PL) of SiOx:H prepared by plasma enhanced chemical vapor deposition has been systematically studied in conjunction with infrared and micro-Raman spectra. We have found that each PL spectrum is comprised of two Gaussian components, a main band and a shoulder. The main band might originate from amorphous silicon clusters embedded in the SiOx network, and its redshift with annealing temperature is due to expansion of the silicon clusters. The shoulder remains at about 835 nm in spite of the annealing temperature and possibly comes from luminescent defect centers. The enhanced PL spectra after 1170 °C annealing are attributed to the quantum confinement effects of nanocrystalline silicon embedded in the SiO2 matrix.

Hali tarjima qilinmagan

Identifikatorlar

Iqtiboslar va manbalar

3 ta iqtibos0 ta foydalanilgan manba