Дилафруз КурбановаJizzakh Polytechnic Institute (Uzbekistan)Sanobar BobomurodovaJizzakh Polytechnic Institute (Uzbekistan)Normurot FAYZULLAYEVSamarkand State University (Uzbekistan)Shaxlo AripovaTashkent Institute of Textile and Light Industry (Uzbekistan)Kamola UsmanovaJizzakh Polytechnic Institute (Uzbekistan)Sidora KarimovaJizzakh Polytechnic Institute (Uzbekistan)
2026

Ochiq kirish: yoʻq

ABI

Annotatsiya

The work examines the technological characteristics and principal scheme of the process of oxychlorination of ethylene with hydrogen chloride in the presence of atmospheric oxygen. The catalyst KClZnCl2MnCl2*CuCl2/ASC (aluminosilicate carrier) was selected for industrial application, as it demonstrated the best results during the study. The reactor designed for the oxidative chlorination (oxychlorination) reaction of ethylene with hydrogen chloride in the presence of atmospheric oxygen has a height of 32.4 m and a diameter of 3.3 m. The amount of catalyst in the oxychlorination reactor is 55 tons. The process temperature is 212-220 °C, with a temperature difference of 2-3 °C along the height of the catalyst bed. The reaction gas mixture passes through the catalyst bed from bottom to top at a velocity of 0.25-0.35 m/sec. This ensures good interaction between the reaction gas mixture and the catalyst particles. In such reactors, the heat supply ensures that the reaction medium is maintained at a uniform and stable temperature, which serves to increase the selectivity and conversion of the reaction.

Hali tarjima qilinmagan

Identifikatorlar

Iqtiboslar va manbalar

0 ta iqtibos0 ta foydalanilgan manba