Photoluminescence, stacking faults, and carrier transport in n-type 3C-SiC/Si(100) structures grown by endotaxial HT-CVD

B.G. AtabaevInstitute of Ion Plasma Laser TechnologiesM. V. DolgopolovSamara State Technical University, Samara, RussiaKh.N. JuraevNational University of UzbekistanA. S. ChipuraSamara State Technical University, Samara, RussiaВ.И. ЧепурновSamara University, Samara, RussiaR. JalolovLaboratory of Optical and Electron Processes in Nanostructured Materials, U.A. Arifov Institute of Ion-Plasma and Laser Technologies, Uzbekistan Academy of Sciences, Tashkent, UzbekistanO. (Odilbek) TurgunovLaboratory for Growth of Semiconductor Crystals, S.A. Azimov Physical-Technical Institute of Uzbekistan Academy of Sciences, Tashkent, UzbekistanS. A. RadzhapovLaboratory for High Energy Physics, S.A. Azimov Physical-Technical Institute of Uzbekistan Academy of Sciences, Tashkent, UzbekistanZ.Sh. ShaymardanovInstitute of Ion Plasma Laser TechnologiesШ.З. УроловLaboratory of Optical and Electron Processes in Nanostructured Materials, U.A. Arifov Institute of Ion-Plasma and Laser Technologies, Uzbekistan Academy of Sciences, Tashkent, Uzbekistan
2026en

Ochiq kirish: yoʻq

ABI

Annotatsiya

We present a comprehensive study of photoluminescence (PL) and electrical transport in n-type 3C-SiC/Si(100) heterostructures grown by high-temperature chemical vapor deposition (HT-CVD) in an endotaxial regime at 1340–1360 °C. The PL spectrum of sample KEF-32 is deconvoluted into four Gaussian components centered at 385, 433, 511, and 563 nm, which are attributed to near-band-edge (NBE) recombination in strained 3C-SiC, donor–acceptor pair (DAP) transitions, and recombination at stacking faults (SFs) and associative impurity–defect complexes. For sample KEF-32-5, grown at the upper level of the graphite container, the PL spectrum is confined to the 383–464 nm range and lacks a distinct deep-level band at 2.2 eV, indicating a modified role of SF-related centers and a redistribution of recombination away from the current-carrying volume. Hall-effect measurements on samples grown under different hydrocarbon supersaturation (32-2 and 32-5) yield electron concentrations of 8 . 5 × 1 0 16 and 2 . 4 × 1 0 16 cm −3 and mobilities of 461 and 1120 cm 2 /Vs, respectively, at a resistivity of about 0.2 Ω cm. Sample 32-5 operates near the phonon-limited mobility regime, whereas sample 32-2 is dominated by ionized impurity and associated defect scattering. The role of stacking faults and associative impurity–defect complexes in shaping the PL bands and scattering mechanisms is discussed. One-dimensional TCAD simulations, incorporating the measured parameters and effective trap densities, reveal that the reduced doping and optimized defect distribution in sample 32-5 lead to a broader depletion region and lower leakage currents, confirming the improved device potential. The results provide quantitative guidelines for optimizing HT-CVD growth of 3C-SiC/Si(100) for power electronics and quantum applications.

Hali tarjima qilinmagan

Identifikatorlar

Iqtiboslar va manbalar