Predicting the tenacity of an antistatic combined yarn made of cotton and a conductive multifilament: load sharing between the components and the critical mass fraction
Annotatsiya
Antistatic combined yarns, in which a conductive multifilament is twisted with a cotton fibre strand on a ring spinning frame, consist of components that differ greatly in extensibility. This study develops a method for predicting the tenacity of a single combined yarn made of cotton fibre and a conductive multifilament on the basis of load sharing between the components. By combining the formulae of A.G. Kogan, M.N. Belitsin and A.N. Solovyev, a generalised model accounting for two failure modes, rupture of the less extensible component and rupture of the remaining component, is proposed, and the critical mass fraction of the multifilament Xk* = Rs/[Rs + Rk(1 − ε1/ε2)] is derived. For a 24 tex combined yarn based on cotton characterised with the Uster LVI system (mean length 26.09 mm, uniformity 86.1 %, micronaire 4.4) and Nega-Stat® P210, the predicted tenacity was 10.9 cN/tex against 11.3 cN/tex measured, a deviation of 3.5 %. Sensitivity analysis showed that 97.8 % of the yarn tenacity is provided by the cotton component and that the critical fraction for Nega-Stat® P210 is 39.7 %, an extrapolation beyond the 30 % validity limit of Kogan’s formula. Replacing it with a silver-coated polyamide multifilament (Rk = 48.3 cN/tex, 49.1 cN/tex with twist correction; ε2 = 21 %) is calculated to raise the tenacity to 14.5 cN/tex (+33 %). The consistency of the input data of Solovyev’s formula requires verification before the accuracy of the method can be regarded as established.
Hali tarjima qilinmagan