A STUDY ON THE EFFECTS OF TEMPERATURE, TIME FLUSHING AND COMPOSITION OF PRINTING PAINT ON THE THICKENER WASHING-OFF
Feruza Baxodirxonovna IbragimovaCandidate of Technical Sciences, Researcher of Bukhara State University, Uzbekistan, Tashkent city
ABI
Annotatsiya
Developed polymer composition consisting of starch, CMC and sericine as a thickener has the characteristics of the highest washability. At a temperature that equals to 800C, for 40 minutes washing circuit about 75% of thickener formulations of polymeric composition are removed from the fabric, in case of the conventional starch thickener only 10% of thickener formulations are removed.